Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed for automotive snap-fit electronic connectors. It offers high flow and short molding cycles. The processing window is relatively broad and mold temperatures as low as 150°F (65°C) can be used.Features: Good Chemical Resistance; Good Flow; Good Wear Resistance; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Impact Modified; Low Friction; LubricatedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PPA0123 G30 KD150 KN080 PM095 PN095 YI255 LD002 Color: BK-324 Black; ASTM D4000 PPA0123 G30 KD150 KN080 PM095 PN095 YI255 LD002 Color: NT Natural; ASTM D6779 PA103G30; DELPHI MS 5218 Color: BK-324 Black; DELPHI MS 5218 Color: NT Natural; GM GMP.PPA.017 Color: BK-324 Black; GM GMP.PPA.017 Color: NT Natural; GM GMW16363P-PPA-GF30 Color: Black; GM GMW16363P-PPA-GF30 Color: Natural; ISO 1874-PA 6T/66-HI, MH, 11-090, GF30Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Filler Content 30 %
30 %
Glass Fiber
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 167 MPa
24200 psi
ASTM D638
170 MPa
24700 psi
ISO 527-2
Elongation at Break 3.2 %
3.2 %
ASTM D638
3.3 %
3.3 %
ISO 527-2
Tensile Modulus 9.31 GPa
1350 ksi
ISO 527-2
Flexural Strength 225 MPa
32600 psi
ISO 178
Flexural Yield Strength 236 MPa
34200 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ISO 178
7.86 GPa
1140 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Izod Impact, Unnotched 14.0 J/cm
26.2 ft-lb/in
ASTM D256
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
Type 1, Edgewise; ISO 179
Thermal Properties Metric English Comments
Melting Point 306 °C
583 °F
ASTM D3418
310 °C
590 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
HDT B; Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 276 °C
529 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 321 - 335 °C
610 - 635 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Injection Rate Fast
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant