Mechanical Properties Metric English Comments
Shear Modulus 0.0250 - 1.00 GPa

@Temperature 50.0 - 225 °C
3.63 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.688 GPa Grade Count:5
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:7
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..