Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.47 - 1.62 g/cc
0.0531 - 0.0585 lb/in³
Average value: 1.51 g/cc Grade Count:27
Filler Content 15.0 - 20.0 %
15.0 - 20.0 %
Average value: 18.5 % Grade Count:17
Water Absorption 0.180 - 1.60 %
0.180 - 1.60 %
Average value: 0.516 % Grade Count:20
Moisture Absorption at Equilibrium 0.300 - 0.600 %
0.300 - 0.600 %
Average value: 0.500 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00800 cm/cm
0.00100 - 0.00800 in/in
Average value: 0.00335 cm/cm Grade Count:27
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00599 cm/cm Grade Count:4
Melt Flow 6.00 - 43.5 g/10 min
6.00 - 43.5 g/10 min
Average value: 26.2 g/10 min Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98.0 - 125
98.0 - 125
Average value: 118 Grade Count:13
Tensile Strength, Ultimate 81.4 - 150 MPa
11800 - 21800 psi
Average value: 118 MPa Grade Count:23
80.0 - 110 MPa

@Temperature 60.0 - 150 °C
11600 - 16000 psi

@Temperature 140 - 302 °F
Average value: 95.0 MPa Grade Count:1
Tensile Strength, Yield 109 - 133 MPa
15800 - 19300 psi
Average value: 125 MPa Grade Count:5
Elongation at Break 1.50 - 5.00 %
1.50 - 5.00 %
Average value: 2.97 % Grade Count:27
2.60 - 3.00 %

@Temperature 60.0 - 150 °C
2.60 - 3.00 %

@Temperature 140 - 302 °F
Average value: 2.78 % Grade Count:1
Elongation at Yield 2.50 - 2.50 %

@Temperature 150 - 150 °C
2.50 - 2.50 %

@Temperature 302 - 302 °F
Average value: 2.50 % Grade Count:1
Modulus of Elasticity 4.48 - 13.8 GPa
650 - 2000 ksi
Average value: 6.61 GPa Grade Count:24
5.90 - 6.50 GPa

@Temperature 60.0 - 150 °C
856 - 943 ksi

@Temperature 140 - 302 °F
Average value: 6.21 GPa Grade Count:1
Flexural Yield Strength 138 - 193 MPa
20000 - 28000 psi
Average value: 175 MPa Grade Count:22
Flexural Modulus 3.79 - 6.89 GPa
550 - 1000 ksi
Average value: 5.79 GPa Grade Count:22
Compressive Yield Strength 124 - 138 MPa
18000 - 20000 psi
Average value: 131 MPa Grade Count:8
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Izod Impact, Notched 0.320 - 0.854 J/cm
0.600 - 1.60 ft-lb/in
Average value: 0.672 J/cm Grade Count:22
Izod Impact, Unnotched 1.87 - 7.47 J/cm
3.50 - 14.0 ft-lb/in
Average value: 5.99 J/cm Grade Count:16
Izod Impact, Notched (ISO) 6.00 - 6.50 kJ/m²
2.86 - 3.09 ft-lb/in²
Average value: 6.33 kJ/m² Grade Count:3
6.50 - 6.50 kJ/m²

@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 - 4.70 J/cm²
11.9 - 22.4 ft-lb/in²
Average value: 3.85 J/cm² Grade Count:4
4.50 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.400 - 0.650 J/cm²
1.90 - 3.09 ft-lb/in²
Average value: 0.575 J/cm² Grade Count:4
0.650 - 0.650 J/cm²

@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.650 J/cm² Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 20.0 - 39.6 µm/m-°C
11.1 - 22.0 µin/in-°F
Average value: 32.0 µm/m-°C Grade Count:15
23.0 - 23.0 µm/m-°C

@Temperature 140 - 180 °C
12.8 - 12.8 µin/in-°F

@Temperature 284 - 356 °F
Average value: 23.0 µm/m-°C Grade Count:2
Thermal Conductivity 0.190 - 0.303 W/m-K
1.32 - 2.10 BTU-in/hr-ft²-°F
Average value: 0.281 W/m-K Grade Count:8
Maximum Service Temperature, Air 180 - 220 °C
356 - 428 °F
Average value: 199 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 210 - 224 °C
410 - 435 °F
Average value: 217 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 204 - 220 °C
399 - 428 °F
Average value: 211 °C Grade Count:26
Glass Transition Temp, Tg 225 °C
437 °F
Average value: 225 °C Grade Count:3
Flammability, UL94 V-0
V-0
Grade Count:23
Oxygen Index 39.0 - 44.5 %
39.0 - 44.5 %
Average value: 41.6 % Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 200 - 1.00e+17 ohm-cm
200 - 1.00e+17 ohm-cm
Average value: 1.01e+16 ohm-cm Grade Count:22
Surface Resistance 200 - 1.00e+14 ohm
200 - 1.00e+14 ohm
Average value: 7.50e+13 ohm Grade Count:4
Dielectric Constant 3.80 - 4.20
3.80 - 4.20
Average value: 3.90 Grade Count:10
Dielectric Strength 14.8 - 37.0 kV/mm
375 - 940 kV/in
Average value: 18.0 kV/mm Grade Count:15
Dissipation Factor 0.00150 - 0.0100
0.00150 - 0.0100
Average value: 0.00611 Grade Count:10
Arc Resistance 70.0 - 110 sec
70.0 - 110 sec
Average value: 75.6 sec Grade Count:9
Comparative Tracking Index 125 - 150 V
125 - 150 V
Average value: 142 V Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 80.0 - 366 °C
176 - 690 °F
Average value: 320 °C Grade Count:8
Melt Temperature 340 - 399 °C
644 - 750 °F
Average value: 363 °C Grade Count:16
Mold Temperature 93.0 - 190 °C
199 - 374 °F
Average value: 155 °C Grade Count:23
Drying Temperature 135 - 180 °C
275 - 356 °F
Average value: 151 °C Grade Count:15
Moisture Content 0.0400 %
0.0400 %
Average value: 0.0400 % Grade Count:9
Dew Point -31.7 °C
-25.0 °F
Average value: -31.7 °C Grade Count:9
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:16