Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.20 - 2.31 GPa | 319 - 335 ksi | Calculated |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Shear Modulus | 2.20 GPa | 319 ksi | calculated |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Shear Modulus | 2.20 - 4.20 GPa | 319 - 609 ksi | Average value: 3.23 GPa Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |