Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.99 - 4.20 GPa | 579 - 609 ksi | Calculated |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Shear Modulus | 2.20 - 4.20 GPa | 319 - 609 ksi | Average value: 3.23 GPa Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |