Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Shear Modulus | 77.0 GPa @Temperature 20.0 - 100 °C |
11200 ksi @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Shear Modulus | 77.0 GPa @Temperature 20.0 - 100 °C |
11200 ksi @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Shear Modulus | 77.0 GPa @Temperature 20.0 - 100 °C |
11200 ksi @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Shear Modulus | 77.0 GPa @Temperature 20.0 - 100 °C |
11200 ksi @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior .. |
|||
Shear Modulus | 77.0 GPa @Temperature 20.0 - 100 °C |
11200 ksi @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | Calculated |
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Shear Modulus | 77.0 GPa @Temperature 260 °C |
11200 ksi @Temperature 500 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.250 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | torsion |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum 309H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum 310H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Shear Modulus | 77.0 GPa | 11200 ksi | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |