Polymer Property : Film Tensile Strength at Yield, TD = 15.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade
Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin
Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
at 2% offset; ASTM D882
ExxonMobil Pax-Plus™ 3204 Blown Film Resin
Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin..
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
Dow LDPE 768A Low Density Polyethylene, Film Grade
DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a..