Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ.. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1.. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | at 2% offset; ASTM D882 |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |
|||
Film Tensile Strength at Yield, TD | 15.2 MPa | 2200 psi | |
Dow LDPE 768A Low Density Polyethylene, Film Grade DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a.. |