Polymer Property : Film Tensile Strength at Yield, TD = 4800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 33.1 MPa
>= 4800 psi
ASTM D 882 A
Total Finathene® 2344 HDPE film  (discontinued **)
Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D822
LyondellBasell Alathon® L5906 High Density Polyethylene
ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t..
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D882
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu..
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D882
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D828
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D882
ExxonMobil HD 7960.13 HMW Blown Film Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..