Polymer Property : Film Tensile Strength at Yield, TD = 653 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 4.50 MPa
653 psi
ISO 527-3
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Film Tensile Strength at Yield, TD 4.50 MPa
653 psi
ASTM D882
ExxonMobil Escorene® LD-708 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal ..
Film Tensile Strength at Yield, TD 4.50 MPa
653 psi
ISO 527-3
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch ..