Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.10 g/micron | 104 g/mil | ISO 6383-2 |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Elmendorf Tear Strength, TD | 4.10 g/micron | 104 g/mil | ASTM D1922 |