Elmendorf Tear Strength, TD 4.10 g/micron
104 g/mil
ISO 6383-2
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch ..
Elmendorf Tear Strength, TD 4.10 g/micron
104 g/mil
ASTM D1922
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..