Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 22.4 g/micron | 570 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p.. |
|||
Elmendorf Tear Strength, TD | 22.4 g/micron | 570 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove.. |
|||
Elmendorf Tear Strength, TD | 22.4 g/micron | 570 g/mil | ASTM D1922 |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Elmendorf Tear Strength, TD | 22.4 g/micron | 570 g/mil | ASTM D1922 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Elmendorf Tear Strength, TD | 22.4 g/micron | 570 g/mil | ASTM D1922 |
Dow ELITE™ 5500G Enhanced Polyethylene Resin ™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te.. |