Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 7.30 g/micron | 185 g/mil | ASTM D1922 |
Reliance Industries Reclair F18020 Polyethylene Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, an.. |
|||
Elmendorf Tear Strength, TD | 7.30 g/micron | 185 g/mil | |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Elmendorf Tear Strength, TD | 7.30 g/micron | 185 g/mil | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Elmendorf Tear Strength, TD | 7.30 g/micron | 185 g/mil | |
Dow LDPE 752A Low Density Polyethylene, Film Grade DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu.. |
|||
Elmendorf Tear Strength, TD | 7.30 - 27.6 g/micron | 185 - 701 g/mil | Average value: 16.8 g/micron Grade Count:11 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |