Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 682I Low Density Polyethylene, Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 682I Low Density Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Thickness 40.0 microns
1.57 mil
Melt Flow 0.70 g/10 min

@Load 2.16 kg
0.70 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1490 psi
Film Tensile Strength at Yield, TD 10.3 MPa
1490 psi
Film Elongation at Break, MD 360 %
360 %
Film Elongation at Break, TD 530 %
530 %
Coefficient of Friction 0.70
0.70
Elmendorf Tear Strength MD 270 g
270 g
Elmendorf Tear Strength TD 290 g
290 g
Elmendorf Tear Strength, MD 6.80 g/micron
173 g/mil
Elmendorf Tear Strength, TD 7.30 g/micron
185 g/mil
Dart Drop 3.50 g/micron
88.9 g/mil
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
Film Tensile Strength at Break, TD 19.3 MPa
2800 psi
Optical Properties Metric English Comments
Haze 8.5 %
8.5 %
Gloss 64 %
64 %
45°
Processing Properties Metric English Comments
Processing Temperature 218 °C
424 °F
Film extrusion temperature