Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 051.LT Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Dart Drop Test | 180 g | 0.397 lb | 50 microns film |
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 113 Low Density Polyethylene IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Arkema Group OREVAC® 9307 Y EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |
|||
Dart Drop Test | 180 g | 0.397 lb | |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Global J-4324 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |