Mechanical Properties Metric English Comments
Dart Drop Test 110 g
0.243 lb
ASTM D1709
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Dart Drop Test >= 110 g
>= 0.243 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test >= 110 g
>= 0.243 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test 110 g
0.243 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a..
Dart Drop Test 110 g
0.243 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze..
Dart Drop Test 110 g
0.243 lb
F<sub>50</sub>, Estimated from TEDD value of 0.3 ft-lbs. For standard dart and 26" drop height.; ASTM D1709
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film)
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b..
Dart Drop Test 110 g
0.243 lb
Cast; ASTM D1709, F<sub>50</sub>
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Dart Drop Test 110 g
0.243 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA952000 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Dart Drop Test 110 g
0.243 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA952094 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Dart Drop Test 110 g
0.243 lb
ASTM D1709
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film
Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena..
Dart Drop Test 110 g
0.243 lb
Cast; ASTM D1709, F<sub>50</sub>
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Dart Drop Test 110 g
0.243 lb
ASTM D1709
Westlake EF1807 Low Density Polyethylene
Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA ..
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
Westlake EN1817AA Low Density Polyethylene
Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli..
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin
Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America..
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl..
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Dart Drop Test 110 g
0.243 lb
Film; 50.8 microns; ASTM D1709A
Dow DX5E66 Polypropylene Homopolymer Resin
OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P..
Dart Drop Test 110 g
0.243 lb
g/F50; ASTM D1709
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability..
Dart Drop Test 110 g
0.243 lb
ASTM-D1709
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer
LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p..
Dart Drop Test 110 g
0.243 lb
g/F50; ASTM D1709
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene
Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability...