Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Film Tensile Strength at Break, TD 90.0 MPa

@Thickness 0.100 mm
13100 psi

@Thickness 0.00394 in
ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Film Tensile Strength at Break, TD 90.0 - 350 MPa
13100 - 50800 psi
Average value: 180 MPa Grade Count:3
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ASTM D882
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6
Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6
Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6
Information provided by EMS Grivory
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6
Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6
Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6
Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® F 40 NL PA6
Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® F 47 NL nat 6028 PA6
Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai..
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..
Copyright © lookpolymers.com All Rights Reserved