Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 33.8 MPa | 4900 psi | ASTM D882 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Break, TD | 33.8 MPa | 4900 psi | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Film Tensile Strength at Break, TD | 33.8 MPa | 4900 psi | |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |
|||
Film Tensile Strength at Break, TD | 33.8 MPa | 4900 psi | ASTM D882 |
ExxonMobil Escorene® LD 721.IK Film Resin Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,.. |
|||
Film Tensile Strength at Break, TD | 33.8 MPa | 4900 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |