Polymer Property : Film Tensile Strength at Break, TD = 3600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Petrothene® NA362176 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
LyondellBasell Petrothene® NA362005 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
Westlake LF1020 Butene Linear Low Density Polyethylene
Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
Westlake LF1021 Butene Linear Low Density Polyethylene
Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend ..