Film Tensile Strength at Break, TD 262 MPa
38000 psi
ASTM D882
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade
Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
510
ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film
Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high ene..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 612LLG102 OPP Film
Product Description: A clear, two-side treated, polypropylene film that is used in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. 612..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte® 50 TSPM OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized a one-side treated. TSP< is designed for use as the inner web of a cold seal lamination or as the center web of a t..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 12MM281 OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
ASTM D882A
DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge
Melinex® D316 is a polyester film designed for the label industry, one side pretreated to promote adhesion to a wide variety of solventless, UV, EB, and thermal cured coatings.Adhesion promoting on..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
ASTM D882A
DuPont Teijin Films Mylar® SR Polyester Film
Mylar® SR is a developmental film being produced to provide an economical substrate for use in thin, clear film applications such as post lamination or silicone release applications. The product is..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
JIS C-2318 (Modified to TDF)
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 ..
Film Tensile Strength at Break, TD 262 MPa
38000 psi
510
ExxonMobil Label-Lyte® 612 LL-112 Clear OPP Overlaminate
Clear, polypropylene film designed to provide exceptional clarity and print protection when used as an overlaminate in pressure-sensitive labeling applications. The treated high energy layer provide..