Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 1184 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527 |
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | 2 in per min; ASTM D882 |
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | Calculated from mfr's report of 49 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | |
Dow HDPE 05862N High Density Polyethylene Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Film Tensile Strength at Break, TD | 28.0 - 50.0 MPa | 4060 - 7250 psi | Average value: 42.2 MPa Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | ASTM D882 |
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **) Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc.. |
|||
Film Tensile Strength at Break, TD | 28.0 MPa | 4060 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **)< 18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |