Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 34.5 - 55.2 MPa | 5000 - 8000 psi | ASTM D882 |
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Film Tensile Strength at Break, TD | 34.5 - 55.2 MPa | 5000 - 8000 psi | ASTM D882 |
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |