Film Tensile Strength at Break, TD 34.5 - 55.2 MPa
5000 - 8000 psi
ASTM D882
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide..
Film Tensile Strength at Break, TD 34.5 - 55.2 MPa
5000 - 8000 psi
ASTM D882
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide..