Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble..
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags..
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 3.1 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng..
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 3 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,..
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..