Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East) LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific) XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Yield Strength | 100 - 147 MPa | 14500 - 21300 psi | Average value: 128 MPa Grade Count:8 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | ASTM D790 |
Techmer ES Plaslube® NY-1/TF/13/SI/2 Nylon 66, 13% PTFE, 2% Silicone Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | ASTM Data |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Conditioned)