Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ISO METHOD 176 |
NYCOA 2047 Copolymer Nylon 6/69 extrusion, high melt viscosity. & strength., low crystallinity Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Nylene® Norpex® AX245 PPE (Polyphenylene Ether) Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Flexural Yield Strength | 71.0 - 255 MPa | 10300 - 37000 psi | Average value: 130 MPa Grade Count:176 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
LG Chemical HI-121 ABS, High Impact Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL003 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech CastAlloy Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech Crylex High Impact Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 71.1 MPa @Thickness 6.40 mm |
10300 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |