Spartech SolarKote® /ABS Weatherable Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylic (PMMA)
Manufacturer Spartech
Trade Name SolarKote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SolarKote® /ABS Weatherable Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Tensile Modulus 1.79 GPa
260 ksi
ASTM D638
Flexural Yield Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Unnotched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
0.534 J/cm

@Temperature -40.0 °C
1.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 27.1 J
20.0 ft-lb
73°F; ASTM D3029
10.8 J

@Temperature -40.0 °C
8.00 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523