Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 46.9 - 85.5 MPa | 6800 - 12400 psi | Average value: 64.8 MPa Grade Count:11 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |