Polymer Property : Flexural Yield Strength = 6800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 46.9 MPa
6800 psi
ASTM D790
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 29% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Flexural Yield Strength 46.9 MPa
6800 psi
ASTM D790
Westlake Plastics Kynar® 2850 PVDF Copolymer
Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab..
Flexural Yield Strength 46.9 MPa
6800 psi
ASTM D790
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate
Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 46.9 - 85.5 MPa
6800 - 12400 psi
Average value: 64.8 MPa Grade Count:11
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..