Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 13.0 - 170 MPa @Temperature 125 - 275 °C |
1890 - 24700 psi @Temperature 257 - 527 °F |
Average value: 72.2 MPa Grade Count:2 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 69.0 - 170 MPa | 10000 - 24700 psi | Average value: 89.8 MPa Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Yield Strength | 96.5 - 170 MPa | 14000 - 24700 psi | Average value: 129 MPa Grade Count:8 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Flexural Yield Strength | 32.0 - 170 MPa | 4640 - 24700 psi | Average value: 86.9 MPa Grade Count:184 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |