Mechanical Properties Metric English Comments
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min; ASTM D790
Ovation Polymers Opnyl OP66GF43 Nylon 66, Dry as Molded
Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min; ASTM D790
Ovation Polymers RIGITRON 20433 GF PBT, 33% Glass Reinforced
PBT - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco..
Flexural Yield Strength 185 MPa

@Temperature 90.0 °C
26800 psi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar..
Flexural Yield Strength 185 MPa
26800 psi
ISO 178, ASTM D790
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens)
Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ..
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev..
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati..
Flexural Yield Strength 185 MPa
26800 psi
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Flexural Yield Strength 185 MPa
26800 psi
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT
LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber.
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT
LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Flexural Yield Strength 185 MPa
26800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East)
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East)
LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength
Flexural Yield Strength 185 MPa
26800 psi
ISO 178
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Flexural Yield Strength 185 MPa
26800 psi
ISO 178
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
Eurostar Starflam RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding ResinInformation provided by Eurostar.
Flexural Yield Strength 185 MPa
26800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.