Mechanical Properties Metric English Comments
Flexural Yield Strength 189 MPa
27400 psi
DIN 53452; ASTM D790
Kolon Kopa® KN153G30 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Flexural Yield Strength 189 MPa
27400 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific)
30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif..
Flexural Yield Strength 189 MPa
27400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific)
LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, ..