Material Notes:
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent chemical resistance, Wide usage temperature, Good impact absorbing characteristics. Information provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.13 %
0.13 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
DIN 53505; ASTM D785
Tensile Strength, Ultimate 133 MPa
19300 psi
DIN 53455; ASTM D638
Elongation at Break 5.0 %
5.0 %
DIN 53455; ASTM D638
Flexural Yield Strength 189 MPa
27400 psi
DIN 53452; ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 1.47 J/cm
2.75 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149/DIN 53481
Arc Resistance 123 sec
123 sec
ASTM D495
Users viewing this material also viewed the following: