Mechanical Properties Metric English Comments
Flexural Yield Strength 22.0 MPa
3190 psi
ASTM D790
NYCOA 2011 Copolymer Nylon
impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc.
Flexural Yield Strength 22.0 - 393 MPa
3190 - 57000 psi
Average value: 206 MPa Grade Count:148
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Flexural Yield Strength 22.0 - 65.0 MPa
3190 - 9430 psi
Average value: 42.9 MPa Grade Count:15
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..