Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 95.0 - 220 MPa | 13800 - 31900 psi | Average value: 167 MPa Grade Count:81 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Flexural Yield Strength | 110 - 220 MPa | 16000 - 31900 psi | Average value: 155 MPa Grade Count:21 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 74.5 - 220 MPa | 10800 - 31900 psi | Average value: 151 MPa Grade Count:46 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Flexural Yield Strength | 31.0 - 220 MPa | 4500 - 31900 psi | Average value: 77.7 MPa Grade Count:74 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |