Polymer Property : Flexural Yield Strength = 40000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 4005 SI  Polyphthalamide (PPA) Glass Fiber 30% - Silicone  (discontinued **)
Glass Fiber 30% - SiliconeComments:Glass FiberSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pro..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 2299 X 68910 A  Polyetheretherketone (PEEK) Long Glass Fiber 40%  (discontin
Long Glass Fiber 40%Comments:Long Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 1110  Polyethylene Terephthalate (PET) Glass Fiber 55%  (discontinued **)<
Glass Fiber 55%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 1185  Polyethylene Terephthalate (PET) Carbon Fiber 30%  (discontinued **)&l
Carbon Fiber 30%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
Solvay Specialty Polymers Kadel® E-1230 Polyketone  (discontinued **)
Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 2185 TFE 5  Polyetherimide (PEI) Carbon Fiber 30% - PTFE 5%  (discontinued *
Carbon Fiber 30% - PTFE 5%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 2185 TFE 13 SI 2  Polyetherimide (PEI) Carbon Fiber 30% - PTFE 13% - Silicone 2% &
Carbon Fiber 30% - PTFE 13% - Silicone 2%Comments:Carbon FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can af..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 209D  Nylon 6/12 (PA 6/12) Glass Fiber 50%  (discontinued **)
Glass Fiber 50%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
Techmer ES HiFill® PPS GF40 TL13 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
Techmer ES Plastiblend® PA6 GF30 RM BK Nylon 6
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Flexural Yield Strength 276 MPa
40000 psi
Long Beam, dry
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric
Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber
Data provided by Clariant Masterbatches
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 284C  Nylon 11 (PA 11) Carbon Fiber 25%  (discontinued **)
Carbon Fiber 25%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 285D TFE 13 SI 2  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 13% - Silicone 2% &
Carbon Fiber 30% - PTFE 13% - Silicone 2%Comments:Carbon FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can af..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 208B  Nylon 6/10 (PA 6/10) Glass Fiber 45%  (discontinued **)
Glass Fiber 45%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 285B TFE 13 SI 2  Nylon 6/10 (PA 6/10) Carbon Fiber 30% - PTFE 13% - Silicone 2% &
Carbon Fiber 30% - PTFE 13% - Silicone 2%Comments:Carbon FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can af..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 209E  Amorphous Nylon (Am. PA) Glass Fiber 50%  (discontinued **)
Glass Fiber 50%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 3999X56542B Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant  (discontinued **)
Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 283E  Amorphous Nylon (Am. PA) Carbon Fiber 20%  (discontinued **)
Carbon Fiber 20%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 1389 HEC  Polyphenylene Sulfide (PPS) Nickel-Coated Carbon Fiber 50% - EMI/ESD &n
Nickel-Coated Carbon Fiber 50% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 4082A  Polyphthalamide - Hot Water Mold (PPA) Carbon Fiber 15%  (discontinue
Carbon Fiber 15%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Flexural Yield Strength 276 - 303 MPa
40000 - 44000 psi
Average value: 290 MPa Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% ..
Flexural Yield Strength 276 MPa
40000 psi
ASTM D790
RTP Company RTP 4008A FR  Polyphthalamide - Hot Water Mold (PPA) Electronic Encapsulation - 45% Glass Fiber - Flame Retardant
Electronic Encapsulation - 45% Glass Fiber - Flame RetardantComments:Encapsulation GradeGlass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored material..