Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 41.2 MPa | 5980 psi | 15 mm/min; ASTM D790 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |