Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 17.0 - 70.0 MPa | 2470 - 10200 psi | Average value: 42.9 MPa Grade Count:163 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |