Polymer Property : Flexural Yield Strength = 2470 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 17.0 MPa
2470 psi
ASTM D790
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
Flexural Yield Strength 17.0 - 70.0 MPa
2470 - 10200 psi
Average value: 42.9 MPa Grade Count:163
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Flexural Yield Strength 17.0 - 48.3 MPa
2470 - 7000 psi
Average value: 35.7 MPa Grade Count:43
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Flexural Yield Strength 17.0 - 340 MPa

@Temperature -40.0 - 250 °C
2470 - 49300 psi

@Temperature -40.0 - 482 °F
Average value: 105 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Flexural Yield Strength 17.0 - 340 MPa

@Thickness 0.800 - 3.17 mm
2470 - 49300 psi

@Thickness 0.0315 - 0.125 in
Average value: 105 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Flexural Yield Strength 17.0 - 507 MPa
2470 - 73500 psi
Average value: 79.8 MPa Grade Count:236
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 17.0 MPa
2470 psi
at 3.5%
Biomer P240 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Flexural Yield Strength 17.0 - 183 MPa

@Temperature -40.0 - 120 °C
2470 - 26500 psi

@Temperature -40.0 - 248 °F
Average value: 85.1 MPa Grade Count:12
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Flexural Yield Strength 17.0 - 105 MPa
2470 - 15200 psi
Average value: 37.7 MPa Grade Count:54
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Flexural Yield Strength 17.0 - 51.7 MPa
2470 - 7500 psi
Average value: 29.7 MPa Grade Count:27
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Flexural Yield Strength 17.0 - 110 MPa
2470 - 16000 psi
Average value: 36.9 MPa Grade Count:38
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler