Mechanical Properties Metric English Comments
Flexural Yield Strength 74.0 - 92.0 MPa
10700 - 13300 psi
Average value: 81.2 MPa Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..