Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D 882 |
NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ISO 527-3 |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM-D882 |
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene Frozen chicken packages; Meat-based frozen packages.Additives: Antiblock, D, PPA, PEBDInformation provided by Braskem. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM-D882 |
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM-D882 |
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM-D882 |
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
1% Secant Modulus, MD | 180 MPa | 26100 psi | ASTM D882 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |