Material Notes:
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly for reuse on the same surface or application to another surface.Information provided by 3M
Physical Properties Metric English Comments
Thickness 81.3 microns
3.20 mil
Liner
102 microns
4.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.0219 kN/m
0.125 pli
Bond Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.0219 kN/m
0.125 pli
Bond Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.0219 kN/m
0.125 pli
Glass, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.0219 kN/m
0.125 pli
Cellaphane, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.027391 kN/m
0.15625 pli
Cellaphane, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.027391 kN/m
0.15625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.03287 kN/m
0.1875 pli
Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.03287 kN/m
0.1875 pli
Painted Metal, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.03287 kN/m
0.1875 pli
Glass, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.03287 kN/m
0.1875 pli
Polypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.03287 kN/m
0.1875 pli
Painted Metal, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.03287 kN/m
0.1875 pli
Acrylic, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
0.05478 kN/m
0.3125 pli
Acrylic, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.0877 kN/m
0.500 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
-15.0 °C
5.00 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 1000 repositionable acrylic
Liner 50# densified kraft
Users viewing this material also viewed the following: