Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.386 kN/m | 2.20 pli | PVC vs. PVC, 15 minutes |
Taiwan PU Corporation TPUA-760 TPU Shoe Adhesive A PU resin for general application with excellent adhesion to all kinds of media.Features: Fast crystallization rateGood initial adhesionGood thermo toleranceCan be used alone or combined with a cro.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7250 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | Polypropylene, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP027202 White Polypropylene Label Product 3M™ White Polypropylene Label Product FP027202 is a glossy white opaque material that offers excellent durability and moisture resistance. This label product utilizes 3M™ Adhesive P1400, which is .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFL0208 Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M OFM0103 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M OFM0202 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M OFM0202N-60 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM03402 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0402 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0702 Outdoor UL Recognized Brite Silver Polyester Label Products 3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM1602 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM1702 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7225 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7237 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1400, which is a high performance tackified acry.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7238 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7242 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1400, which is a high performance tackified acry.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | Bond Strength; Arlon SQA -TMS-015 |
Arlon 910-10W##-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, White, Rectangular cross-section, Self-fu.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M OFM010N Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0403 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0405 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0802 Outdoor UL Recognized Brite Silver Polyester Label Products 3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM0805 Outdoor UL Recognized Brite Silver Polyester Label Products 3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM1502 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFM1605 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV02610N Textured Vinyl Label Products 3M™ Textured Vinyl Label Product FV02610N is a flexible and conformable clear vinyl label stock that offers durability and moisture resistance. This vinyl label utilizes 3M™ Adhesive P1400, which .. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFL010N Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFL0202 Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |
|||
Peel Strength | 0.386 kN/m | 2.20 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M OFL020N Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |