Polymer Property : Peel Strength = 0.95319 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.95319 kN/m
5.4375 pli
to stainless steel, 90°, 72 hr at 70°C; ASTM D3330
3M 444 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
Peel Strength 0.95319 kN/m
5.4375 pli
to stainless steel, 90°, 72 hr at 70°C; ASTM D3330
3M 444PC Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
Peel Strength 0.95319 kN/m
5.4375 pli
to Stainless Steel, 90°, 2 mil Al foil, 72 hr at 70°C; ASTM D3330
3M 9589 Double Coated Tapes with Adhesive 700 Series
3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat..