Polymer Property : Peel Strength = 1.10 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.193 kN/m
1.10 pli
Bond Strength; Arlon SQA -TMS-011
Arlon 66211A007 0.007" (0.178 mm) Uncured Silicone Rubber Monofilament Polyester Fabric Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Monofilament Polyester Fabric Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represent..
Peel Strength 0.193 - 0.228 kN/m
1.10 - 1.30 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive
4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Remova..
Peel Strength 0.193 kN/m
1.10 pli
Bond Strength; Arlon SQA-TMS-011
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate
Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum..
Peel Strength 0.193 kN/m
1.10 pli
Aluminum
3M Fastbond™ 100 Lavender Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..
Peel Strength 0.193 kN/m
1.10 pli
Galvanized Steel
3M Fastbond™ 100 Lavender Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..
Peel Strength 0.193 kN/m
1.10 pli
Cold Rolled
3M Fastbond™ 100 Lavender Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..
Peel Strength 0.193 kN/m
1.10 pli
Aluminum
3M Fastbond™ 100 Neutral Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..
Peel Strength 0.193 kN/m
1.10 pli
Galvanized Steel
3M Fastbond™ 100 Neutral Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..
Peel Strength 0.193 kN/m
1.10 pli
Cold Rolled
3M Fastbond™ 100 Neutral Foam Adhesive
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t..