Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 825 MPa @Temperature 23.0 °C |
120000 psi @Temperature 73.4 °F |
|
Special Metals NIMONIC® Alloy 86 A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°.. |
|||
Tensile Strength, Ultimate | 825 MPa @Temperature 23.0 °C |
120000 psi @Temperature 73.4 °F |
|
Special Metals INCONEL® Alloy HX A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high.. |