Polymer Property : Tensile Modulus = 2.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.80 GPa

@Temperature 150 °C
406 ksi

@Temperature 302 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Tensile Modulus 2.80 GPa

@Temperature 23.0 °C
406 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Tensile Modulus 2.80 GPa

@Temperature 60.0 °C
406 ksi

@Temperature 140 °F
LATI Lapex A PES
Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Tensile Modulus 2.80 GPa

@Temperature 23.0 °C
406 ksi

@Temperature 73.4 °F
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 2.80 GPa

@Temperature 90.0 °C
406 ksi

@Temperature 194 °F
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
Tensile Modulus 2.80 GPa

@Temperature 23.0 °C
406 ksi

@Temperature 73.4 °F
LATI Latamid 6 BH PA 6, Heat Stabilized
Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
Tensile Modulus 2.80 GPa

@Temperature 150 °C
406 ksi

@Temperature 302 °F
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 2.80 GPa

@Temperature 150 °C
406 ksi

@Temperature 302 °F
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 2.80 GPa

@Temperature 90.0 °C
406 ksi

@Temperature 194 °F
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Tensile Modulus 2.80 GPa

@Temperature 150 °C
406 ksi

@Temperature 302 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Tensile Modulus 2.80 GPa

@Temperature 23.0 °C
406 ksi

@Temperature 73.4 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Tensile Modulus 2.80 GPa

@Temperature 150 °C
406 ksi

@Temperature 302 °F
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..
Tensile Modulus 2.80 GPa

@Temperature 90.0 °C
406 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..