Polymer Property : Tensile Modulus = 3190 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 22.0 GPa

@Temperature 60.0 °C
3190 ksi

@Temperature 140 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 22.0 GPa

@Temperature 23.0 °C
3190 ksi

@Temperature 73.4 °F
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &..
Tensile Modulus 22.0 GPa

@Temperature 120 °C
3190 ksi

@Temperature 248 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Modulus 22.0 GPa

@Temperature 60.0 °C
3190 ksi

@Temperature 140 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 22.0 GPa

@Temperature 120 °C
3190 ksi

@Temperature 248 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 22.0 GPa

@Temperature 150 °C
3190 ksi

@Temperature 302 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Modulus 22.0 GPa

@Temperature 71.0 °C
3190 ksi

@Temperature 160 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel
Tensile Modulus >= 22.0 GPa

@Temperature 50.0 °C
>= 3190 ksi

@Temperature 122 °F
ISO 527-2
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..