Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.90 GPa @Temperature 90.0 °C |
856 ksi @Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.90 GPa @Temperature 150 °C |
856 ksi @Temperature 302 °F |
|
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 5.90 GPa @Temperature 23.0 °C |
856 ksi @Temperature 73.4 °F |
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 5.90 GPa @Temperature 60.0 °C |
856 ksi @Temperature 140 °F |
|
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |